I am currently running some tests on it now, I just tried on my N2+ for the first time last week and I had very weak layers and my outer shells actually peeled right off. I will let you know what works for PETG on the Pro2 once I can get it dialed in.
-
- Posts: 31
- Joined: Mon May 07, 2018 4:07 pm
Re: PETG on Pro2
Just finished a test cube with the standard PETG settings for the Pro2. Came out pretty well, much better than my print on the N2. the layers are very well bonded, there is some light stringing between pieces but not bad. I did not use a raft and it stuck to the buildtak very well with the bed distance set at 0.2 using the supplied feeler gauge.
Re: PETG on Pro2
I read that almost everyone recommends high temperatures with PETG.
I on the pro2 with the PETG the best result I get it with temperature 210/215 °, speed 40 mm/s, layer 0.2
I on the pro2 with the PETG the best result I get it with temperature 210/215 °, speed 40 mm/s, layer 0.2
Re: PETG on Pro2
I use PETG most of the time, I love it. I print straight onto a glass sheet at 260C & 80C. It sticks really well for printing and then releases easily when the bed cools below 30C. The bottom face comes out with a mirror-like finish.
Re: PETG on Pro2
PETG temps depend on the brand and color - I print small vase-mode test parts at different temps to find the best layer-bonding strength. Usually lands between 240C and 270C.